中空玻璃打胶机胶枪堵塞的解决方案!

浏览:0
  中空玻璃胶枪胶枪卡壳的解决方案,要进行故障排除,有针对性地进行解决。
  To solve the problem of the shell of the glue gun of the hollow glass glue gun, we must first remove the trouble and solve it pertinently.
  主要问题如下:
  The main problems are as follows:
  胶粘剂氧化引起的堵塞。
  First adhesive oxidation caused by plugging.
  第二胶中杂质太多
  Too many impurities in the second glue
  第三,它没有被清理
  Third, it has not been cleaned up
  随着市场竞争的日益激烈,一些厂家使用含有大量杂质的劣质硅胶胶,长期使用导致中空玻璃胶机胶枪堵塞,该怎么办?
  With the increasingly fierce market competition, some manufacturers use a lot of impurities in the poor quality silica gel glue, long-term use leads to the blocking of hollow glass glue machine gun, what should be done?
  中空玻璃打浆机胶枪堵塞原因:
  Reasons for blocking of glue gun of hollow glass beater:
  1. 在上胶过程中,中间中断时间长,或累计多次,施胶结束时清洗不彻底,特别是在夏季温度较高时,胶水固化快。
  1. In the process of sizing, the intermediate interruption time is long, or accumulated many times, and the cleaning is not complete at the end of sizing, especially in summer when the temperature is high, the glue solidifies quickly.
  2. AB组分气压不足,混合不均匀,出胶慢,容易产生颗粒。
  2. The air pressure of AB component is insufficient, the mixture is uneven, the glue is slow, and particles are easy to be produced.
  3.B组件没有检查和清洁。B组分对水蒸气很敏感。由于运输、储存环境等偶发因素,B组分的结皮可能发生在表面,当结皮部分被压入管道时,容易产生颗粒
  3. B components are not inspected and cleaned. Component B is very sensitive to water vapor. Due to the occasional factors such as transportation and storage environment, the crust of component B may occur on the surface, and when the crust part is pressed into the pipeline, it is easy to produce particles
济南双组份打胶机
  4. 滤网和单向止回阀很久没有清洗了。
  4. The filter screen and check valve have not been cleaned for a long time.
  5. B组件压力板上的o形环使用时间长,已经松动。
  5. The O-ring on the pressure plate of B-component has been loose for a long time.
  中空玻璃胶机胶枪堵塞解决方案:
  Solution for blocking the glue gun of hollow glass glue machine:
  1 .胶料的断胶时间应多长,建议在断胶前,断胶时间应根据每天前不同的温度和湿度而定。另外,现在客户经常要求胶液固化时间快,中断时间长一点容易造成颗粒的出现。
  1. How long should the breaking time of rubber compound be? It is suggested that before breaking, the breaking time should be determined according to the different temperature and humidity of the day before each day. In addition, customers often require fast curing time and longer interruption time, which is easy to cause particles.
  2 .简单处理是用刮板刮去外壳,不影响胶水的使用。
  2. The simple treatment is to scrape off the shell with a scraper without affecting the use of glue.
  建议定期清洗过滤器、单向止回阀、静电混合器和胶枪。
  It is recommended to clean the filter, one-way check valve, electrostatic mixer and glue gun regularly.